Sugar cane hammers with better service life

Allgemeine Information
Name des Centers
SSAB
Beschreibung des Kundenbeispiels

Description: Second Step crushing in a sugar mill

Technical data: Wear from the frictional heat on the head of the cap. A squeezing / crushing action needed for the fragmentation

Service Life and Status: Hard faced mild steel hammer held one week. New design with shaft in Hardox 400 and cap in Hardox 600 holds two weeks.

Further Service life increases will be achieved by a HF(Hard facing) layer on top of the Hardox 600 cap.  A butter layer of austenitic 307 is needed.

Endkunde
Branche
Landwirtschaft, Forstwirtschaft, Fischerei
Verarbeitete Rohmaterialien
Grains
Verschleißteil
Ausrüstung
Hammers
Temperatur
0 – 250 °C / 32 – 480 °F
Verarbeitete Materialgröße
10 – 300 mm / 0,4 – 12,0 "
Lösung
Neue Lösung
Hardox 600
Wichtige Erfolgsfaktoren
Optimierte Lebensdauer
+30 %